VINYL CHARACTERISTIC CHART

VINYL PROPERTIES

TEST METHOD

RESULTS
Base Fabric  

9 x 9 1000 D. Polyester
Weight  

14 oz. p.s.y.
Embossing  

Crush
Adhesion

5970

20 lbs./2 inch
Tear Strength

5134 (Warp x Fill)

75 Warp x 75 Fill
Tensile Strength

5100 (Warp x Fill)

220 Warp x 220 Fill
Flame Resistance

5903 (Warp x Fill)

-
After Flame  

2 Sec. x 2 Sec.
Char Length  

4 Sec. x 4 Sec.
The above figures represent typical data and are subject to slight variations. These figures are not intended to be used as specifications.